Characterization of Five Different Implant Surfaces and Their Effect on Osseointegration: A Study in Dogs
Autor(es): 
Instituição: 
  • NYU
  • UNIGRANRIO Univ Sch Hlth Sci
  • Universidade Estadual Paulista (UNESP)
  • Universidade Federal de Santa Catarina (UFSC)
  • Tufts Univ
ISSN: 
0022-3492
Resumo: 
Background: Chemical modification of implant surface is typically associated with surface topographic alterations that may affect early osseointegration. This study investigates the effects of controlled surface alterations in early osseointegration in an animal model.Methods: Five implant surfaces were evaluated: 1) alumina-blasting, 2) biologic blasting, 3) plasma, 4) microblasted resorbable blasting media (microblasted RBM), and 5) alumina-blasting/acid-etched (AB/AE). Surface topography was characterized by scanning electron microscopy and optical interferometry, and chemical assessment by x-ray photoelectron spectroscopy. The implants were placed in the radius of six dogs, remaining 2 and 4 weeks in vivo. After euthanization, specimens were torqued-to-interface failure and non-decalcified - processed for histomorphologic bone-implant contact, and bone area fraction-occupied evaluation. Statistical evaluation was performed by one-way analysis of variance (P < 0.05) and post hoc testing by the Tukey test.Results: The alumina-blasting surface presented the highest average surface roughness and mean root square of the surface values, the biologic blasting the lowest, and AB/AE an intermediate value. The remaining surfaces presented intermediate values between the biologic blasting and AB/AE. The x-ray photoelectron spectroscopy spectra revealed calcium and phosphorus for the biologic blasting and microblasted RBM surfaces, and the highest oxygen levels for the plasma, microblasted RBM, and AB/AE surfaces. Significantly higher torque was observed at 2 weeks for the microblasted RBM surface (P < 0.04), but no differences existed between surfaces at 4 weeks (P > 0.74). No significant differences in bone-implant contact and bone area fraction-occupied values were observed at 2 and 4 weeks.Conclusion: The five surfaces were osteoconductive and resulted in high degrees of osseointegration and biomechanical fixation. J Periodontol 2011;82:742-750.
Data de publicação: 
1-Mai-2011
Citação: 
Journal of Periodontology. Chicago: Amer Acad Periodontology, v. 82, n. 5, p. 742-750, 2011.
Duração: 
742-750
Publicador: 
Amer Acad Periodontology
Palavras-chaves: 
  • Animal
  • bone
  • dental implant
  • histology
  • osseointegration
  • torque
Fonte: 
http://dx.doi.org/10.1902/jop.2010.100520
Endereço permanente: 
Direitos de acesso: 
Acesso restrito
Tipo: 
outro
Fonte completa:
http://repositorio.unesp.br/handle/11449/16015
Aparece nas coleções:Artigos, TCCs, Teses e Dissertações da Unesp

Não há nenhum arquivo associado com este item.
 

Itens do Acervo digital da UNESP são protegidos por direitos autorais reservados a menos que seja expresso o contrário.