Title: 
Mechanochemical synthesis of barium titanate
Author(s): 
Institution: 
  • University of Belgrade
  • Universidade Estadual Paulista (UNESP)
  • Univ Nis
ISSN: 
0955-2219
Abstract: 
A powder mixture of BaO and TiO2, was mechanochemically treated in a planetary ball mill in an air atmosphere for up to 4 h, using zirconium oxide vial and zirconium oxide balls as the milling medium. Mechanochemical reaction leads to the gradual formation of BaTiO3 phase. Phase evolution during synthesis and changes in powder size and morphology were monitored by XRD, DSC, IR and TEM analysis and it was shown that the formation of BaTiO3 phase was initiated after 60 min. Extended time of milling directed to formation of higher amount of BaTiO3 perovskite phase. Barium titanate with good crystallinity was formed after 240 min sintering without pre-calcination step was performed at 1330 degrees C for 2 It within heating rate 10 degrees C/min. (c) 2005 Elsevier Ltd. All rights reserved.
Issue Date: 
1-Jan-2005
Citation: 
Journal of the European Ceramic Society. Oxford: Elsevier B.V., v. 25, n. 12, p. 1985-1989, 2005.
Time Duration: 
1985-1989
Publisher: 
Elsevier B.V.
Keywords: 
barium titanate
Source: 
http://dx.doi.org/10.1016/j.jeurceramsoc.2005.03.003
URI: 
Access Rights: 
Acesso restrito
Type: 
outro
Source:
http://repositorio.unesp.br/handle/11449/36525
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.