Você está no menu de acessibilidade

Utilize este identificador para citar ou criar um link para este item: http://acervodigital.unesp.br/handle/11449/8482
Título: 
Powder Diffraction of Components Subject to Corrosion in Fuse Cutouts with CeramicInsulation
Autor(es): 
Instituição: 
Universidade Estadual Paulista (UNESP)
ISSN: 
0255-5476
Resumo: 
Aiming identification of the components most affected by corrosion under saline environment conditions, we have carried out X-ray diffraction measurements in ceramic and bond materials, all in the powder form. The ceramic is analyzed before and after thermal annealing at 1000 degrees C, showing the same DRX peaks, although better defined after annealing. Identification suggests the presence of Al(6)Si(2)O(13) (Mullite) and SiO(2) (Quartz). Analysis of the junction (bond) material shows similar peaks, but a metallic preponderance is observed. Thermal annealing of the junction is done at much lower temperature, because it melts in the range 135 degrees C-170 degrees C, when a whitish smoke begins to show up along with strong sulfur odor.
Data de publicação: 
1-Jan-2008
Citação: 
Advanced Powder Technology Vi. Stafa-zurich: Trans Tech Publications Ltd, v. 591-593, p. 548-553, 2008.
Duração: 
548-553
Publicador: 
Trans Tech Publications Ltd
Palavras-chaves: 
  • Fuse cutouts
  • X-ray diffraction
  • ceramic
  • mullite
  • corrosion
Fonte: 
http://dx.doi.org/10.4028/www.scientific.net/MSF.591-593.548
Endereço permanente: 
http://hdl.handle.net/11449/8482
Direitos de acesso: 
Acesso restrito
Tipo: 
outro
Fonte completa:
http://repositorio.unesp.br/handle/11449/8482
Aparece nas coleções:Artigos, TCCs, Teses e Dissertações da Unesp