Effects of substituting ytterbium for scandium on the microstructure and age-hardening behaviour of Al-Sc alloy
Author(s): 
Institution: 
  • Univ Minho
  • Universidade Estadual Paulista (UNESP)
ISSN: 
0921-5093
Sponsorship: 
  • Project Bridging The Gap
  • Erasmus Mundus External Cooperation Window Program
Abstract: 
In order to reduce the cost of Al-Sc alloys and maintain their mechanical properties, the microstructure and mechanical properties of Al-0.24 wt% Sc-0.07 wt% Yb in comparison with Al-0.28 wt% Sc alloys were studied. The aging behaviour, precipitate morphologies, precipitate coarsening and precipitation hardening of both alloys were investigated. The average diameter and the size distribution of nanoscale Al3Sc and Al-3(Sc,Yb) precipitates at various aging conditions were measured. Transmission electron microscopy (TEM) and high-resolution TEM were used to deeply understand the precipitate evolution. A maximum hardness around 73 (HV30) was obtained with a precipitate diameter from 4.3 to 5.6 nm for both alloys. (c) 2014 Elsevier B.V. All rights reserved.
Issue Date: 
17-Apr-2014
Citation: 
Materials Science And Engineering A-structural Materials Properties Microstructure And Processing. Lausanne: Elsevier Science Sa, v. 601, p. 70-77, 2014.
Time Duration: 
70-77
Publisher: 
Elsevier B.V.
Keywords: 
  • Aluminium-scandium alloys
  • Ytterbium
  • Age-hardening
  • Precipitate coarsening
  • TEM
  • High-resolution TEM
Source: 
http://dx.doi.org/10.1016/j.msea.2014.02.042
URI: 
Access Rights: 
Acesso restrito
Type: 
outro
Source:
http://repositorio.unesp.br/handle/11449/111705
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.