Title: 
Effect of surface treatment on the bond strength between yttria partially stabilized zirconia ceramics and resin cement
Author(s): 
Institution: 
  • Universidade Estadual Paulista (UNESP)
  • Universidade Federal Fluminense (UFF)
  • Universidade de São Paulo (USP)
ISSN: 
0022-3913
Sponsorship: 
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Sponsorship Process Number: 
CNPq: 150922/2011-6
Abstract: 
Statement of problem. No consensus has been reached on the best bonding protocol between a zirconia ceramic surface and the tooth structure.Purpose. The purpose of this study was to evaluate the extrusion shear strength between yttria partially stabilized zirconia ceramics and resin cement (Panavia F) after different surface treatments.Material and methods. The surface treatments evaluated (n=7) included the following: G1-control group (no surface treatment); G2-treated with MDP primer (Alloy Primer); G3-treated with 40% hydrofluoric acid (210 seconds); and G4-treated with 40% hydrofluoric acid (210 seconds) followed by MDP primer. The specimens were bonded to 2.5-mm-thick disks of bovine root dentin, and the extrusion shear tests were performed after they had been stored for 24 hours in distilled water at 37 degrees C. The surface modifications were assessed on 2 specimens that were selected from each group by scanning electron microscopy. Data were analyzed with 1-way ANOVA and the Tukey-Kramer honestly significant difference test (alpha=.05).Results. G4 (mean 2.84, standard deviation [SD] 0.43 MPa) presented significantly higher (P<.001) extrusion shear strength when compared with the other groups in the study (G1: mean, 1.57; SD 0.28 MPa; G2: mean 1.46, SD 0.28 MPa; G4: mean 1.16, SD 0.41 MPa). No significant differences were found among the other groups in the study.Conclusions. Yttria partially stabilized zirconia ceramics can be treated with 40% hydrofluoric acid for 210 seconds to increase the bond strength with the resin cement.
Issue Date: 
1-Aug-2014
Citation: 
Journal Of Prosthetic Dentistry. New York: Mosby-elsevier, v. 112, n. 2, p. 357-364, 2014.
Time Duration: 
357-364
Publisher: 
Elsevier B.V.
Source: 
http://dx.doi.org/10.1016/j.prosdent.2013.08.025
URI: 
Access Rights: 
Acesso restrito
Type: 
outro
Source:
http://repositorio.unesp.br/handle/11449/116719
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.