Processamento de cerâmicas reticuladas a partir de matérias-primas naturais
Other Titles: 
Processing of reticulated ceramics using natural raw material
Author(s): 
Institution: 
  • Universidade Federal da Paraíba (UFPB)
  • Universidade Federal do Rio Grande do Norte (UFRN)
  • Universidade Estadual Paulista (UNESP)
ISSN: 
0366-6913
Sponsorship: 
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Abstract: 
  • Foram produzidas cerâmicas porosas reticuladas a partir de uma matéria-prima natural (AF) empregada na produção de telhas e tijolos, misturando-a com caulim (AC). A matéria-prima AF é constituída basicamente de quartzo e feldspatos. O método empregado para confecção das peças cerâmicas foi o da impregnação em espuma polimérica. Foram otimizadas as viscosidades de barbotinas contendo 70% m/m, utilizando poliacrilato de sódio (PAA-Na) como defloculante. As suspensões com 70% m/m de AF apresentaram viscosidade em torno de 600 mPa.s, reduzindo para 300 mPa.s após adição de 20% m/m de AC. O teor de PAA-Na empregado para a fabricação das cerâmicas porosas foi 2,0% m/m. A tixotropia e a pseudoplastia das barbotinas facilitaram a impregnação de espumas poliméricas com 5, 10 e 40 poros/cm. As cerâmicas reticuladas foram obtidas após sinterização a 1100 e 1200 ºC. Os difratogramas de raios X indicaram a dissolução do quartzo a 1200 ºC, com uma peça apresentando basicamente mulita e fase vítrea. As cerâmicas reticuladas com porosidade 10 poros/cm apresentaram estrutura suficientemente rígida com resistência mecânica superior a 1,70 MPa e com constante de permeabilidade darciana na ordem de 3,58.10-9 (±10,0%) m².
  • Porous reticulated ceramics were obtained using a natural raw material (AF) usually employed in the production of tiles and bricks, with kaolinite (AC) addition. The AF raw material is constituted of quartz and feldspar. Ceramic pieces were processed using the polymeric sponge impregnation. Viscosities of the slurries with 70% of solids (wt./wt.) were optimized using sodium polyacrilate (PAA-Na) as deffloculant. Suspensions without AC addition presented a viscosity of 600 mPa.s, decreasing to 300 mPa.s after addition of 20% (wt./wt.) AC. The optimized amount of PAA-Na was 2.0% (wt./wt.). Tixotropy and pseudoplasty of the slurries made the impregnation process easier. Polymeric sponges of 5, 10 and 40 pores/cm were used. Ceramic pieces were sintered at 1100 and 1200 ºC. X-ray diffractograms indicated the quartz dissolution at 1200 ºC, leading to a material composed of mullite and vitreous phase. Reticulated ceramics with a porosity of 10 pores/cm presented a rigid structure with mechanical strength higher than 1.70 MPa, with darcian permeability constant of about 3.58 x 10-9 (±10.0 %) m².
Issue Date: 
1-Jun-2006
Citation: 
Cerâmica. Associação Brasileira de Cerâmica, v. 52, n. 322, p. 185-192, 2006.
Time Duration: 
185-192
Publisher: 
Associação Brasileira de Cerâmica
Keywords: 
  • cerâmica reticulada
  • matérias-primas naturais
  • espuma polimérica
  • traditional ceramics
  • shaping
  • suspensions
  • clays
  • functional applications
Source: 
http://dx.doi.org/10.1590/S0366-69132006000200011
URI: 
Access Rights: 
Acesso aberto
Type: 
outro
Source:
http://repositorio.unesp.br/handle/11449/30021
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.