- Barium strontium titanate powder obtained by polymeric precursor method
- Universidade Estadual Paulista (UNESP)
- 1044-5803
- Pure barium strontium titanate powder, with Ba/Sr ratio of 80/20 was prepared by the polymeric precursor method (also called Pechini process). The powder was obtained after a calcination at 800 degreesC for 8 h and characterized by XRD, IR, BET and SEM. The requirements to avoid barium carbonate as a secondary phase are presented and discussed in detail. (C) 2003 Elsevier B.V. All rights reserved.
- 1-Mar-2003
- Materials Characterization. New York: Elsevier B.V., v. 50, n. 2-3, p. 217-221, 2003.
- 217-221
- Elsevier B.V.
- BST
- polymeric precursor
- Pechini
- microstructure
- BET
- http://dx.doi.org/10.1016/S1044-5803(03)00095-0
- Acesso restrito
- outro
- http://repositorio.unesp.br/handle/11449/37139