- Rugosidade superficial de ligas com alto conteúdo de cobre, em função do aquecimento acima da temperatura de fusão.
- Surface roughness of high copper alloys as a function of heating above casting temperature
- Universidade Estadual Paulista (UNESP)
- 0101-1774
- Being the surface roughness a fundamental property in the fit of the castings, it was determined the roughness of 5 high-copper casting alloys, according to the heating over their melting temperature. That way, the specimens made with smooth plastic in the shape of a rectangular plate, 2 mm x 7 mm x 11 mm were invested into a cristobalite investment. After heating and elimination on the plastic, the molds were filled by 3 g of molten alloy, casted in a electrical casting machine at the casting temperature at 25 degrees C and 50 degrees C overheating. The surface roughness was measured in a roughness analyser, Talysurf. As a result, it was verified that there is a variation of surface roughness among the alloys tested, and the heating of the alloys until 50 degrees C over the melting temperature does not interfere in the roughness.
- 1-Dec-1990
- Revista de Odontologia da UNESP, v. 19, n. 1, p. 203-209, 1990.
- 203-209
- copper
- dental alloy
- denture
- surface property
- temperature
- Copper
- Dental Alloys
- Dental Casting Technique
- English Abstract
- Support, Non-U.S. Gov't
- Surface Properties
- Temperature
- http://www.revodontolunesp.com.br/articles/view/id/51ae4a9b1ef1faca3d0021af
- Acesso aberto
- outro
- http://repositorio.unesp.br/handle/11449/64064
There are no files associated with this item.
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.