Abstract: 
Aim: The aim of this in vitro study was to evaluate the surface roughness of three glass ionomer cements (GICs) indicated for ART restorations. Methods: Ten cylindrical specimens of three commercial glass ionomers cements (Vidrion R - S.S. White, Maxxion R - FGM and Vitromolar DFL) were prepared (n=30) without surface finishing or protection. Twenty-four hours after preparation, the surface roughness measurements were obtained as the mean of three readings of the surface of each specimen by profilometry. The roughness values (Ra, μm) were subjected to one-way ANOVA and Tukey's test (p<0.05). Results: No statistically significant differences were observed between Vidrion R (0.18 ± 0.05) and Vitromolar (0.21 ± 0.05), whereas Maxxion R presented significantly higher roughness values than those of the other materials. Conclusions: It may be concluded that characteristics of particle size and composition of the different GICs affected their surface roughness 24 h after preparation.
Issue Date: 
1-Apr-2010
Citation: 
Brazilian Journal of Oral Sciences, v. 9, n. 2, p. 77-80, 2010.
Time Duration: 
77-80
Keywords: 
  • ART
  • Glass ionomer cements
  • Profilometry
  • Restorative dental materials
  • Roughness
Source: 
http://www.bibliotecadigital.unicamp.br/document/?code=43874
URI: 
Access Rights: 
Acesso aberto
Type: 
outro
Source:
http://repositorio.unesp.br/handle/11449/71641
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.