You are in the accessibility menu

Please use this identifier to cite or link to this item: http://acervodigital.unesp.br/handle/11449/116469
Full metadata record
DC FieldValueLanguage
dc.contributor.authorPontes, D. S. L.-
dc.contributor.authorPontes, F. M.-
dc.contributor.authorCapeli, R. A.-
dc.contributor.authorGarzim, M. L.-
dc.contributor.authorChiquito, A. J.-
dc.contributor.authorLongo, E.-
dc.date.accessioned2015-03-18T15:53:21Z-
dc.date.accessioned2016-10-25T20:24:51Z-
dc.date.available2015-03-18T15:53:21Z-
dc.date.available2016-10-25T20:24:51Z-
dc.date.issued2014-09-01-
dc.identifierhttp://dx.doi.org/10.1016/j.ceramint.2014.05.052-
dc.identifier.citationCeramics International. Oxford: Elsevier Sci Ltd, v. 40, n. 8, p. 13363-13370, 2014.-
dc.identifier.issn0272-8842-
dc.identifier.urihttp://hdl.handle.net/11449/116469-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/116469-
dc.description.abstractPerovskite ferroelectric Pb0.60Ca0.20Sr0.20TiO3, Pb0.50Ca0.25Sr0.25TiO3 and Pb0.40Ca0.30Sr0.30TiO3, thin films were deposited on Pt/Ti/SiO2/Si and (1 0 0) LaAlO3 substrates by a chemical solution deposition method. XRD revealed the formation of pure thin films on both substrates. All thin films have very flat surfaces, and no droplets were found on their surfaces. Raman data showed a gradual phase transition from tetragonal to a pseudocubic perovskite structure in these thin films; a simultaneous increase in Ca and Sr contents at room temperature was also observed. Temperature-dependent dielectric permittivity measurements revealed a decreasing ferroelectric-to-paraelectric phase transition temperature with increasing Ca and Sr contents. At 100 kHz, ferroelectric-to-paraelectric phase transition temperatures were approximately 505, 355 and 290 K for Pb0.60Ca0.20Sr0.20TiO3, Pb0.50Ca0.25Sr0.25TiO3 and Pb0.40Ca0.30Sr0.30TiO3 thin films, respectively. The E-g of the films were estimated from Tauc's law and were found to be inversely dependent on the Ca and Sr content amounts. (C) 2014 Elsevier Ltd and Techna Group S.r.l. All rights reserved.en
dc.description.sponsorshipFundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)-
dc.description.sponsorshipConselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)-
dc.description.sponsorshipCoordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)-
dc.format.extent13363-13370-
dc.language.isoeng-
dc.publisherElsevier B.V.-
dc.sourceWeb of Science-
dc.subjectThin filmsen
dc.subjectOptical transmittanceen
dc.subjectChemical synthesisen
dc.subjectPhase transitionen
dc.titleStructural, ferroelectric, and optical properties of Pb0.60Ca0.20Sr0.20TiO3, Pb0.50Ca0.25Sr0.25TiO3 and Pb0.40Ca0.30Sr0.30TiO3 thin films prepared by the chemical solution deposition techniqueen
dc.typeoutro-
dc.contributor.institutionUniversidade Federal de São Carlos (UFSCar)-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.contributor.institutionUniversidade de São Paulo (USP)-
dc.description.affiliationUniv Fed Sao Carlos, Dept Chem, LIEC, BR-13565905 Sao Paulo, Brazil-
dc.description.affiliationUniv Estadual Paulista Unesp, Dept Chem, BR-17033360 Sao Paulo, Brazil-
dc.description.affiliationUniv Sao Paulo, Inst Fis Sao Carlos, BR-13560250 Sao Paulo, Brazil-
dc.description.affiliationUniv Fed Sao Carlos, NanO LaB, Dept Phys, BR-13565905 Sao Paulo, Brazil-
dc.description.affiliationUniv Estadual Paulista Unesp, Inst Chem, Sao Paulo, Brazil-
dc.description.affiliationUnespUniv Estadual Paulista Unesp, Dept Chem, BR-17033360 Sao Paulo, Brazil-
dc.description.affiliationUnespUniv Estadual Paulista Unesp, Inst Chem, Sao Paulo, Brazil-
dc.identifier.doi10.1016/j.ceramint.2014.05.052-
dc.identifier.wosWOS:000340321300096-
dc.rights.accessRightsAcesso restrito-
dc.relation.ispartofCeramics International-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.