You are in the accessibility menu

Please use this identifier to cite or link to this item: http://acervodigital.unesp.br/handle/11449/128906
Full metadata record
DC FieldValueLanguage
dc.contributor.authorFraga, Sara-
dc.contributor.authorValandro, Luiz F.-
dc.contributor.authorBottino, Marco A.-
dc.contributor.authorMay, Liliana G.-
dc.date.accessioned2015-10-21T13:15:24Z-
dc.date.accessioned2016-10-25T21:06:26Z-
dc.date.available2015-10-21T13:15:24Z-
dc.date.available2016-10-25T21:06:26Z-
dc.date.issued2015-07-01-
dc.identifierhttp://www.sciencedirect.com/science/article/pii/S0109564115001141-
dc.identifier.citationDental Materials. Oxford: Elsevier Sci Ltd, v. 31, n. 7, p. E131-E140, 2015.-
dc.identifier.issn0109-5641-
dc.identifier.urihttp://hdl.handle.net/11449/128906-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/128906-
dc.description.abstractObjective. To evaluate the effects of hard machining, glaze firing and hydrofluoric acid etching on the biaxial flexural strength and roughness of a CAD/CAM leucite glass-ceramic; to investigate if ceramic post-machining surface roughness is influenced by the machining order and by the pair of burs used for it.Methods. A hundred forty four discs were machined by six nominally identical pairs of burs and divided into groups (n = 24): (1) machining-M, (2) machining and glaze firing-MG, (3) machining and hydrofluoric acid etching-MA, (4) machining, glaze firing and hydrofluoric acid etching-MGA, (5) machining followed by polishing, as a control-MP, (6) machining, polishing and hydrofluoric acid etching-MPA. The roughness after each treatment (R-a, and R-z) was measured. The discs were submitted to a piston-on-three ball flexure test (ISO 6872/2008) and strength data analyzed through Weibull statistics (95% CI).Results. M resulted in lower characteristic strength (sigma(0)) (128.2 MPa) than MP (177.2 MPa). The glaze firing reduced sigma(0) (109 MPa), without affecting roughness. Hydrofluoric acid etching increased the roughness without affecting sigma(0) Spearman's coefficient (r(s)) indicated strong and significant correlation between machining order and roughness (r(s)R(a) = -0.66; r(s)R(Z), = -0.73). The ceramic post-machining surface roughness differed significantly according to the pair of burs employed (p < 0.05).Significance. hard machining and glaze firing reduced the leucite ceramic strength, while hydrofluoric acid etching did not affect the strength. Variability in the roughness might be expected after machining, since it was influenced by the machining order and by the bur pairing. (C) 2015 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.en
dc.description.sponsorshipPIPE ARD from Federal University of Santa Maria-
dc.description.sponsorshipCoordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)-
dc.format.extentE131-E140-
dc.language.isoeng-
dc.publisherElsevier B.V.-
dc.sourceWeb of Science-
dc.subjectMachiningen
dc.subjectLeucite glass-ceramicen
dc.subjectCAD/CAMen
dc.subjectHydrofluoric acid etchingen
dc.subjectGlaze firingen
dc.subjectBiaxial flexural strengthen
dc.titleHard machining, glaze firing and hydrofluoric acid etching: Do these procedures affect the flexural strength of a leucite glass-ceramic?en
dc.typeoutro-
dc.contributor.institutionUniversidade Federal de Santa Maria (UFSM)-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.description.affiliationDental Science Post Graduate Program, Federal University of Santa Maria, Santa Maria, RS, Brazil-
dc.description.affiliationDepartment of Restorative Dentistry, Federal University of Santa Maria, Santa Maria, RS, Brazil-
dc.description.affiliationUnespSão Paulo State University, Department of Dental Materials and Prosthodontics, São José dos Campos, SP, Brazil-
dc.identifier.doihttp://dx.doi.org/10.1016/j.dental.2015.04.005-
dc.identifier.wosWOS:000355811900001-
dc.rights.accessRightsAcesso restrito-
dc.relation.ispartofDental Materials-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp