You are in the accessibility menu

Please use this identifier to cite or link to this item: http://acervodigital.unesp.br/handle/11449/130573
Full metadata record
DC FieldValueLanguage
dc.contributor.authorSantos, C.-
dc.contributor.authorKelly, C. A.-
dc.contributor.authorRibeiro, S.-
dc.contributor.authorStrecker, K.-
dc.contributor.authorSouza, J. V. C.-
dc.contributor.authorSilva, O. M. M.-
dc.date.accessioned2014-05-20T15:24:45Z-
dc.date.accessioned2016-10-25T21:21:29Z-
dc.date.available2014-05-20T15:24:45Z-
dc.date.available2016-10-25T21:21:29Z-
dc.date.issued2007-07-06-
dc.identifierhttp://dx.doi.org/10.1016/j.jmatprotec.2007.01.015-
dc.identifier.citationJournal of Materials Processing Technology, v. 189, n. 1-3, p. 138-142, 2007.-
dc.identifier.issn0924-0136-
dc.identifier.urihttp://hdl.handle.net/11449/130573-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/130573-
dc.description.abstractThe objective of this work was the obtaining in situ of alpha-SiAlON-SiC composite, using an alternative rare-earth oxide mixture, RE2O3, as sintering additive, by two different sintering processes. As sintering additive, 20 vol.% of AlN-RE2O3 in a molar ratio of 90: 10 was mixed to the alpha-Si3N4 powder. In the Si3N4-AlN-RE2O3 powder mixture, 0, 10, 15 and 20wt.% of SiC were added. The powder batches were milled, dried and compacted by cold isostatic pressing. Two different sintering processes were used: gas-pressure sintering at 1950 degrees C for 1 h under 1.5 MPa of N-2 atmosphere, or uniaxial hot-pressing at 1750 degrees C, for 30 min under pressure of 20 MPa. The sintered samples were characterized by X-ray diffraction, scanning electron microscopy and mechanical properties. XRD patterns indicate only alpha-SiAlON (alpha') and beta-SiC as crystalline phases. It was observed that the SiC addition did not influence the alpha-SiAlON formation, although the growth of elongated alpha'-grains is substantially decreased. The hot-pressed composites presented better mechanical properties, exhibiting fracture toughness of 5 MPa m(1/2) and hardness around 21.5 GPa. (c) 2007 Elsevier B.V. All rights reserved.en
dc.format.extent138-142-
dc.language.isoeng-
dc.publisherElsevier B.V.-
dc.sourceScopus-
dc.subjectalfa-SiAlON-SiC composite-
dc.subjectMechanical properties-
dc.subjectMicrostructure-
dc.subjectSintering processes-
dc.subjectFracture toughness-
dc.subjectGrain growth-
dc.subjectHot pressing-
dc.subjectRare earth additions-
dc.subjectScanning electron microscopy-
dc.subjectSilicon carbide-
dc.subjectSintering-
dc.subjectX ray diffraction-
dc.subjectCold isostatic pressing-
dc.subjectMolar ratio-
dc.subjectUniaxial hot pressing-
dc.subjectComposite materials-
dc.titlealpha-SiAlON-SiC composites obtained by gas-pressure sintering and hot-pressingen
dc.typeoutro-
dc.contributor.institutionUniversidade de São Paulo (USP)-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.contributor.institutionCTA IAE AMR-
dc.description.affiliationUSP EEL, Polo Urbo-Industrial, Gleba AI-6 s/n, Lorena-SP, CEP 12600-000-
dc.description.affiliationFEG-UNESP, Av. Dr. A. Ferreira da Cunha, 333, Guaratingueta, SP CEP 12516-410-
dc.description.affiliationCTA-IAE AMR, Pca Marechal do Ar Eduardo Gomes, 50, S.J. Campos- SP CEP 12228-904-
dc.description.affiliationUnespFEG-UNESP, Av. Dr. A. Ferreira da Cunha, 333, Guaratingueta, SP CEP 12516-410-
dc.identifier.doi10.1016/j.jmatprotec.2007.01.015-
dc.identifier.wosWOS:000246326700016-
dc.rights.accessRightsAcesso restrito-
dc.relation.ispartofJournal of Materials Processing Technology-
dc.identifier.scopus2-s2.0-34147183152-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.