You are in the accessibility menu

Please use this identifier to cite or link to this item: http://acervodigital.unesp.br/handle/11449/16462
Full metadata record
DC FieldValueLanguage
dc.contributor.authorArioli Filho, João Neudenir-
dc.contributor.authorButignon, Luis Eduardo-
dc.contributor.authorPereira, Rodrigo de Paula-
dc.contributor.authorLucas, Matheus Guilherme-
dc.contributor.authorMollo Junior, Francisco de Assis-
dc.date.accessioned2014-05-20T13:46:29Z-
dc.date.available2014-05-20T13:46:29Z-
dc.date.issued2011-05-01-
dc.identifierhttp://www.scielo.br/scielo.php?script=sci_arttext&pid=S1678-77572011000300013&lng=en&nrm=iso&tlng=en-
dc.identifier.citationJournal of Applied Oral Science. Bauru-sp: Univ São Paulo Fac Odontologia Bauru, v. 19, n. 3, p. 249-253, 2011.-
dc.identifier.issn1678-7757-
dc.identifier.urihttp://hdl.handle.net/11449/16462-
dc.description.abstractDenture fractures are common in daily practice, causing inconvenience to the patient and to the dentists. Denture repairs should have adequate strength, dimensional stability and color match, and should be easily and quickly performed as well as relatively inexpensive. Objective: The aim of this study was to evaluate the flexural strength of acrylic resin repairs processed by different methods: warm water-bath, microwave energy, and chemical polymerization. Material and methods: Sixty rectangular specimens (31x10x2.5 mm) were made with warm water-bath acrylic resin (Lucitone 550) and grouped (15 specimens per group) according to the resin type used to make repair procedure: 1) specimens of warm water-bath resin (Lucitone 550) without repair (control group); 2) specimens of warm water-bath resin repaired with warm water-bath; 3) specimens of warm water-bath resin repaired with microwave resin (Acron MC); 4) specimens of warm water-bath resin repaired with autopolymerized acrylic resin (Simplex). Flexural strength was measured with the three-point bending in a universal testing machine (MTS 810 Material Test System) with load cell of 100 kgf under constant speed of 5 mm/min. Data were analyzed statistically by Kruskal-Wallis test (p<0.05). Results: The control group showed the best result (156.04 +/- 1.82 MPa). Significant differences were found among repaired specimens and the results were decreasing as follows: group 3 (43.02 +/- 2.25 MPa), group 2 (36.21 +/- 1.20 MPa) and group 4 (6.74 +/- 0.85 MPa). Conclusion: All repaired specimens demonstrated lower flexural strength than the control group. Repairs with autopolymerized acrylic resin showed the lowest flexural strength.en
dc.format.extent249-253-
dc.language.isoeng-
dc.publisherUniversidade de São Paulo (USP), Faculdade de Odontologia de Bauru-
dc.sourceWeb of Science-
dc.subjectFlexural strengthen
dc.subjectDenture fractureen
dc.subjectDenture repairen
dc.titleFlexural strength of acrylic resin repairs processed by different methods: water bath, microwave energy and chemical polymerizationen
dc.typeoutro-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.description.affiliationSão Paulo State Univ, Araraquara Dent Sch, Dept Dent Mat & Prosthodont, Araraquara, SP, Brazil-
dc.description.affiliationUnespSão Paulo State Univ, Araraquara Dent Sch, Dept Dent Mat & Prosthodont, Araraquara, SP, Brazil-
dc.identifier.wosWOS:000291055000013-
dc.rights.accessRightsAcesso aberto-
dc.identifier.fileS1678-77572011000300013.pdf-
dc.relation.ispartofJournal of Applied Oral Science-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.