You are in the accessibility menu

Please use this identifier to cite or link to this item: http://acervodigital.unesp.br/handle/11449/16473
Full metadata record
DC FieldValueLanguage
dc.contributor.authorRibeiro, Daniela Garcia-
dc.contributor.authorPavarina, Ana Claudia-
dc.contributor.authorMachado, Ana Lucia-
dc.contributor.authorGiampaolo, Eunice Teresinha-
dc.contributor.authorVergani, Carlos Eduardo-
dc.date.accessioned2014-05-20T13:46:31Z-
dc.date.accessioned2016-10-25T17:00:14Z-
dc.date.available2014-05-20T13:46:31Z-
dc.date.available2016-10-25T17:00:14Z-
dc.date.issued2008-11-01-
dc.identifierhttp://www.quintpub.com/journals/qi/abstract.php?article_id=3559#.UjDRzsZwp5I-
dc.identifier.citationQuintessence International. Hanover Park: Quintessence Publishing Co Inc, v. 39, n. 10, p. 833-840, 2008.-
dc.identifier.issn0033-6572-
dc.identifier.urihttp://hdl.handle.net/11449/16473-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/16473-
dc.description.abstractObjectives: To evaluate the effect of microwave disinfection on the flexural strength and Vickers hardness of 4 autopolymerized resins (Kooliner [K], Tokuso Rebase Fast [T], Ufi Gel Hard [U], and New Truliner [N]) and 1 denture base resin (Lucitone 550 [L]). Method and Materials: For each material, 48 specimens (64 x 10 x 3.3 mm) were made and divided into 6 equal groups (n = 8). In the control group, specimens were untreated. Before testing, specimens were immersed in 200 mL of distilled water and submitted to disinfection for 1 of the following irradiation times: 1, 2, 3, 4, or 5 minutes. The irradiation procedure was performed twice. The flexural strength was determined using a testing machine MTS-810 and measurements of Vickers hardness were made on Micromet 2100. The values were submitted to ANOVA and Tukey's test (P = .05). Results: The K material showed a significant increase (P = .0010) in flexural strength following 5 minutes of disinfection compared to control specimens. The flexural strength mean values of materials T, U, and N were not significantly affected (P > .05) by disinfection. Compared to the control group, the K material showed a significant increase in hardness (P < .001) following disinfection for 3, 4, and 5 minutes. For material U, disinfection for 4 and 5 minutes produced specimens with significantly increased hardness values (P < .001) compared to the control group. For material N, disinfection for 5 minutes resulted in significantly higher hardness values (P < .001) than the control group. Conclusion: Regardless of the irradiation time, the flexural strength and hardness of the materials evaluated were not detrimentally affected by microwave disinfection. (Quintessence Int 2008;39:833-840)en
dc.description.sponsorshipFundação para o Desenvolvimento da UNESP (FUNDUNESP)-
dc.format.extent833-840-
dc.language.isoeng-
dc.publisherQuintessence Publishing Co Inc-
dc.sourceWeb of Science-
dc.subjectacrylic resinsen
dc.subjectcross infectionen
dc.subjectdisinfectionen
dc.subjectflexural strengthen
dc.subjecthardnessen
dc.subjectmicrowaveen
dc.titleFlexural strength and hardness of reline and denture base acrylic resins after different exposure times of microwave disinfectionen
dc.typeoutro-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.description.affiliationSão Paulo State Univ, UNESP, Fac Odontol Araraquara, Araraquara Dent Sch,Dept Dent Mat & Prosthodont, BR-14801903 São Paulo, Brazil-
dc.description.affiliationUnespSão Paulo State Univ, UNESP, Fac Odontol Araraquara, Araraquara Dent Sch,Dept Dent Mat & Prosthodont, BR-14801903 São Paulo, Brazil-
dc.description.sponsorshipIdFUNDUNESP: 00252/03-DFP-
dc.identifier.wosWOS:000261138100007-
dc.rights.accessRightsAcesso restrito-
dc.relation.ispartofQuintessence International-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.