dc.contributor.author | Machado, Ana Lucia | - |
dc.contributor.author | Giampaolo, Eunice Teresinha | - |
dc.contributor.author | Pavarina, Ana Claudia | - |
dc.contributor.author | Jorge, Janaina Habib | - |
dc.contributor.author | Vergani, Carlos Eduardo | - |
dc.date.accessioned | 2014-05-20T13:46:36Z | - |
dc.date.accessioned | 2016-10-25T17:00:17Z | - |
dc.date.available | 2014-05-20T13:46:36Z | - |
dc.date.available | 2016-10-25T17:00:17Z | - |
dc.date.issued | 2012-06-01 | - |
dc.identifier | http://dx.doi.org/10.1111/j.1741-2358.2011.00484.x | - |
dc.identifier.citation | Gerodontology. Hoboken: Wiley-blackwell, v. 29, n. 2, p. E375-E382, 2012. | - |
dc.identifier.issn | 0734-0664 | - |
dc.identifier.uri | http://hdl.handle.net/11449/16506 | - |
dc.identifier.uri | http://acervodigital.unesp.br/handle/11449/16506 | - |
dc.description.abstract | Background: This study evaluated the effect of disinfection by immersion and microwave irradiation on the roughness of one denture base resin (Lucitone-L) and five relining materials, three hard (Tokuyama Rebase II-TR, New Truliner-NT, Ufigel Hard-UH) and two resilient (Trusoft-T, Sofreliner-S).Methods: Fifty specimens were made and divided into groups: CL2 specimens were brushed with 4% chlorhexidine (1 min), immersed in the same solution (10 min) and immersed in water (3 min); MW2 specimens were immersed in water and microwave irradiated (650W; 6 min); CL2 and MW2 specimens were disinfected twice; CL7 and MW7 specimens were submitted to seven cycles using chlorhexidine or microwave irradiation, respectively; W specimens were not disinfected and remained in water (37 degrees C; 7 days).Results: Results were statistically analysed (p = 0.05) and revealed that, at baseline, the highest mean value was observed for T (p < 0.001). Material NT showed increase in roughness after the first (p = 0.003), second (p = 0.001), seventh (p = 0.000) cycles of microwave disinfection and after 7 days of immersion in water (p = 0.033).Conclusions: Resilient liner S presented significant increase in roughness after the second cycle of disinfection with chlorhexidine (p = 0.003). Material T exhibited significantly decreased roughness in group W (p = 0.010), while microwaving produced severe alterations on its surface. | en |
dc.format.extent | E375-E382 | - |
dc.language.iso | eng | - |
dc.publisher | Wiley-Blackwell | - |
dc.source | Web of Science | - |
dc.subject | chemical compounds | en |
dc.subject | denture bases | en |
dc.subject | denture rebasing | en |
dc.subject | microwaves | en |
dc.subject | surface properties | en |
dc.title | Surface roughness of denture base and reline materials after disinfection by immersion in chlorhexidine or microwave irradiation | en |
dc.type | outro | - |
dc.contributor.institution | Universidade Estadual Paulista (UNESP) | - |
dc.contributor.institution | Universidade Estadual de Ponta Grossa (UEPG) | - |
dc.description.affiliation | Univ Estadual Paulista UNESP, Araraquara Dent Sch, Dept Dent Mat & Prosthodont, Araraquara, SP, Brazil | - |
dc.description.affiliation | Universidade Estadual de Ponta Grossa (UEPG), Dept Dent, Maringa, Parana, Brazil | - |
dc.description.affiliationUnesp | Univ Estadual Paulista UNESP, Araraquara Dent Sch, Dept Dent Mat & Prosthodont, Araraquara, SP, Brazil | - |
dc.identifier.doi | 10.1111/j.1741-2358.2011.00484.x | - |
dc.identifier.wos | WOS:000308547000055 | - |
dc.rights.accessRights | Acesso aberto | - |
dc.relation.ispartof | Gerodontology | - |
Appears in Collections: | Artigos, TCCs, Teses e Dissertações da Unesp |
There are no files associated with this item.
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.