Você está no menu de acessibilidade

Utilize este identificador para citar ou criar um link para este item: http://acervodigital.unesp.br/handle/11449/22968
Registro de metadados completo
Campo DCValorIdioma
dc.contributor.authorNagayassu, M. P.-
dc.contributor.authorShintome, L. K.-
dc.contributor.authorArana-Chavez, V. E.-
dc.contributor.authorFava, M.-
dc.date.accessioned2014-05-20T14:05:27Z-
dc.date.accessioned2016-10-25T17:10:47Z-
dc.date.available2014-05-20T14:05:27Z-
dc.date.available2016-10-25T17:10:47Z-
dc.date.issued2011-03-01-
dc.identifierhttp://www.ncbi.nlm.nih.gov/pubmed/21678674-
dc.identifier.citationJournal of Clinical Pediatric Dentistry. Birmingham: Journal Pedodontics Inc, v. 35, n. 3, p. 301-304, 2011.-
dc.identifier.issn1053-4628-
dc.identifier.urihttp://hdl.handle.net/11449/22968-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/22968-
dc.description.abstractThe aim of this study was to evaluate the micro-shear bond strength of 5 adhesive systems to enamel, one single-bottle acid-etch adhesive (O), two self-etching primers (P) and two all-in-one self-etching adhesives (S). Method: Sixty premolar enamel surfaces (buccal or lingual) were ground flat with 400- and 600-grit SiC papers and randomly divided into 5 groups (n=12), according to the adhesive system.. SB2 - Single Bond 2 (O); CSE - Clearfil SE Bond (P); ADS - AdheSE (P); PLP - Adper Prompt L-Pop (S); XE3 - Xeno III (S). Tygon tubing (inner diameter of 0.8mm) restricted the bonding area to obtain the resin composite (Z250) cylinders. After storage in distilled water at 37 degrees C for 24h and thermocycling, micro-shear testing was performed (crosshead speed of 0.5mm/min). Data were submitted to one-way ANOVA and Tukey test (a=5%). Samples were also subjected to stereomicroscopic and SEM evaluations after micro-shear testing. Mean bond strength values (MPa +/- SD) and the results of Tukey test were: SB2: 36.36(+/- 3.34)a; ADS: 33.03(+/- 7.83)a; XE3: 32.76(+/- 5.61)a; CSE: 30.61(+/- 6.68)a; PLP: 22.17(+/- 6.05)b. Groups with the same letter were not statistically different. It can be concluded that no significant difference was there between SB2, ADS, XE3 and CSE, in spite of different etching patterns of these adhesives. Only PLP presented statistically lower bond strengths compared with others. J Clin Pediatr Dent 35(3): 301-304, 2011en
dc.format.extent301-304-
dc.language.isoeng-
dc.publisherJournal Pedodontics Inc-
dc.sourceWeb of Science-
dc.titleMicro-Shear Bond Strength of Different Adhesives to Human Dental Enamelen
dc.typeoutro-
dc.contributor.institutionUniversidade de São Paulo (USP)-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.description.affiliationUniv São Paulo, Sch Dent, Div Oral Biol, BR-05508900 São Paulo, SP, Brazil-
dc.description.affiliationUNESP, Sch Dent Sao Jose dos Campos, Dept Children Clin Dent, Sao Jose Dos Campos, SP, Brazil-
dc.description.affiliationUnespUNESP, Sch Dent Sao Jose dos Campos, Dept Children Clin Dent, Sao Jose Dos Campos, SP, Brazil-
dc.identifier.wosWOS:000290593300011-
dc.rights.accessRightsAcesso restrito-
dc.relation.ispartofJournal of Clinical Pediatric Dentistry-