Você está no menu de acessibilidade

Utilize este identificador para citar ou criar um link para este item: http://acervodigital.unesp.br/handle/11449/25244
Registro de metadados completo
Campo DCValorIdioma
dc.contributor.authorGasparotto, G.-
dc.contributor.authorSimões, Alexandre Zirpoli-
dc.contributor.authorZaghete, M. A.-
dc.contributor.authorPerazolli, L.-
dc.contributor.authorVarela, José Arana-
dc.contributor.authorLongo, Elson-
dc.date.accessioned2014-05-20T14:17:30Z-
dc.date.accessioned2016-10-25T17:39:59Z-
dc.date.available2014-05-20T14:17:30Z-
dc.date.available2016-10-25T17:39:59Z-
dc.date.issued2003-04-01-
dc.identifierhttp://dx.doi.org/10.1590/S0366-69132003000200008-
dc.identifier.citationCerâmica. Associação Brasileira de Cerâmica, v. 49, n. 310, p. 110-115, 2003.-
dc.identifier.issn0366-6913-
dc.identifier.urihttp://hdl.handle.net/11449/25244-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/25244-
dc.description.abstractPós de titanato zirconato de chumbo (PZT) puros e dopados com bário foram obtidos pelo método de precursores poliméricos, conformados uniaxialmente, na forma de cilindros, utilizando 15 MPa, e prensados isostaticamente à 210MPa. Com o objetivo de estudar o comportamento de sinterização os compactos foram divididos em dois lotes. Sendo um sinterizado em um forno acoplado a um dilatômetro até a temperatura de 1300 °C e o outro sinterizado em forno tipo mufla, em sistema fechado, na temperatura de 1100 °C por 4 horas. Verificou-se que a adição do íon bário influencia na cinética de sinterização, na densificação final, na microestrutura e nas propriedades elétricas da cerâmica. A adição de bário aumenta a concentração da fase tetragonal no PZT, em função da substituição do chumbo por bário na rede perovskita. As amostras dopadas com concentrações maiores que 5,0 mol % em bário apresentaram segregação de PbO no contorno de grão, inibindo seu crescimento.pt
dc.description.abstractPure and barium doped lead zirconate titanate powders were obtained by the polymeric precursor method, uniaxially conformed in cylinders form using 15 MPa and pressing isostatically at 210 MPa. In order to study the sintering behaviour, the compacts were divided in two parts. One part was sintered in a dilatometer furnace till 1300 °C and the other one sintered in muffle furnace in the temperature of 1100 °C for 4 hours. It was verified that the addition of barium influences on the sintering kinetics, on the final density, microstructure and electric properties of the ceramics. The addition of barium increases the concentration of the tetragonal phase of PZT due to the substitution of lead by barium in the perovskite lattice. The samples doped with barium concentrations higher than 5.0 mol % leads to the segregation of PbO in the grain boundary, inhibiting grain growth.en
dc.format.extent110-115-
dc.language.isopor-
dc.publisherAssociação Brasileira de Cerâmica-
dc.sourceSciELO-
dc.subjectperovskitapt
dc.subjectsinterizaçãopt
dc.subjectPZTpt
dc.subjectpiezoeletricidadept
dc.subjectperovskiteen
dc.subjectsinteringen
dc.subjectPZTen
dc.subjectpiezoelectricityen
dc.titleSíntese e caracterização da cerâmica PZT dopada com íons báriopt
dc.title.alternativeSynthesis and characterization of barium-doped PZT ceramicsen
dc.typeoutro-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.contributor.institutionUniversidade Federal de São Carlos (UFSCar)-
dc.description.affiliationUNESP Instituto de Química LIEC-
dc.description.affiliationUFSCar Departamento de Química LIEC-
dc.description.affiliationUnespUNESP Instituto de Química LIEC-
dc.identifier.doi10.1590/S0366-69132003000200008-
dc.identifier.scieloS0366-69132003000200008-
dc.rights.accessRightsAcesso aberto-
dc.identifier.fileS0366-69132003000200008.pdf-
dc.relation.ispartofCerâmica-
Aparece nas coleções:Artigos, TCCs, Teses e Dissertações da Unesp

Não há nenhum arquivo associado com este item.
 