You are in the accessibility menu

Please use this identifier to cite or link to this item: http://acervodigital.unesp.br/handle/11449/30032
Full metadata record
DC FieldValueLanguage
dc.contributor.authorScalvi, L. V. A.-
dc.contributor.authorPineiz, T. F.-
dc.contributor.authorPinheiro, M. A. L.-
dc.contributor.authorSaeki, M. J.-
dc.contributor.authorBriois, V.-
dc.date.accessioned2014-05-20T15:16:25Z-
dc.date.accessioned2016-10-25T17:50:13Z-
dc.date.available2014-05-20T15:16:25Z-
dc.date.available2016-10-25T17:50:13Z-
dc.date.issued2011-09-01-
dc.identifierhttp://dx.doi.org/10.1590/S0366-69132011000300019-
dc.identifier.citationCerâmica. Associação Brasileira de Cerâmica, v. 57, n. 343, p. 225-230, 2011.-
dc.identifier.issn0366-6913-
dc.identifier.urihttp://hdl.handle.net/11449/30032-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/30032-
dc.description.abstractIncorporação de Ce3+ ou Ce4+ em filmes finos de SnO2 depositados via sol-gel-dip-coating aumenta drasticamente a resistividade elétrica. No primeiro caso, temos comportamento aceitador do dopante, levando a matriz à alta compensação de carga. Por outro lado, para Ce4+, verifica-se aumento na largura da região de depleção do contorno de grão, resultando em maior espalhamento de elétrons. Medidas de caracterização elétrica sob pressão ambiente levam à barreiras de potencial mais altas do que as medidas sob vácuo, devido a adsorção de oxigênio na superfície das partículas. A presença de Ce3+ aumenta a transmitância no infravermelho, o que significa menor quantidade de elétrons livres. Dados de XANES confirmam que o tratamento térmico a 550 ºC dos filmes, ainda que promova oxidação parcial para Ce4+, preserva uma quantidade significativa (em torno de 60%) no estado Ce3+. Espectroscopia Raman mostra a evolução dos modos de vibração intra-grãos de SnO2 com o aumento da temperatura de tratamento térmico.pt
dc.description.abstractIncorporation of Ce3+ or Ce4+ in sol-gel dip-coating SnO2 thin films increases drastically its electrical resistivity. In the first case, it is due the acceptor-like nature of the doping ion, leading the matrix to high charge compensation. on the other hand, for Ce4+ doped samples, it is verified a broadening of the grain boundary depletion layer. Measurements under room pressure leads to higher intergrain potential barriers when compared to measurements carried out under vacuum conditions, due to oxygen adsorption at particles surface. The presence of Ce3+ increases the infrared transmittance, which means a lower free electron concentration. XANES data confirms that the thermal annealing at 550 ºC of thin films, although promotes oxidation to Ce4+, still keeps a significantly amount (about 60%) of ions in the oxidation state Ce3+. Raman spectroscopy data show the evolution of the SnO2 bulk vibration modes with increasing thermal annealing temperature.en
dc.description.sponsorshipFundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)-
dc.description.sponsorshipConselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)-
dc.description.sponsorshipCoordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)-
dc.format.extent225-230-
dc.language.isopor-
dc.publisherAssociação Brasileira de Cerâmica-
dc.sourceSciELO-
dc.subjectdióxido de estanhopt
dc.subjectfilmes finospt
dc.subjectcériopt
dc.subjectterras-raraspt
dc.subjecttransporte elétricopt
dc.subjecttin dioxideen
dc.subjectthin filmsen
dc.subjectceriumen
dc.subjectrare-earthen
dc.subjectelectrical transporten
dc.titleResistividade do filme depositado via sol-gel e estado de oxidação do dopante Ce na matriz SnO2pt
dc.title.alternativeResistivity of the film deposited via sol-gel and oxidation state of Ce doping in SnO2 matrixen
dc.typeoutro-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.description.affiliationUniversidade Estadual Paulista FC Dep. Física-
dc.description.affiliationUniversidade Estadual Paulista-
dc.description.affiliationUniversidade Estadual Paulista Programa de Pós-Graduação em Ciência e Tecnologia Materiais-
dc.description.affiliationUniversidade Estadual Paulista Instituto de Biociências Dep. Química e Bioquímica-
dc.description.affiliationUnespUniversidade Estadual Paulista FC Dep. Física-
dc.description.affiliationUnespUniversidade Estadual Paulista-
dc.description.affiliationUnespUniversidade Estadual Paulista Programa de Pós-Graduação em Ciência e Tecnologia Materiais-
dc.description.affiliationUnespUniversidade Estadual Paulista Instituto de Biociências Dep. Química e Bioquímica-
dc.identifier.doi10.1590/S0366-69132011000300019-
dc.identifier.scieloS0366-69132011000300019-
dc.rights.accessRightsAcesso aberto-
dc.identifier.fileS0366-69132011000300019.pdf-
dc.relation.ispartofCerâmica-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.