You are in the accessibility menu

Please use this identifier to cite or link to this item: http://acervodigital.unesp.br/handle/11449/39165
Full metadata record
DC FieldValueLanguage
dc.contributor.authorZanetti, S. M.-
dc.contributor.authorSantiago, E. I.-
dc.contributor.authorBulhoes, LOS-
dc.contributor.authorVarela, José Arana-
dc.contributor.authorLeite, E. R.-
dc.contributor.authorLongo, Elson-
dc.date.accessioned2014-05-20T15:29:37Z-
dc.date.accessioned2016-10-25T18:04:52Z-
dc.date.available2014-05-20T15:29:37Z-
dc.date.available2016-10-25T18:04:52Z-
dc.date.issued2003-06-01-
dc.identifierhttp://dx.doi.org/10.1016/S0167-577X(02)01380-0-
dc.identifier.citationMaterials Letters. Amsterdam: Elsevier B.V., v. 57, n. 19, p. 2812-2816, 2003.-
dc.identifier.issn0167-577X-
dc.identifier.urihttp://hdl.handle.net/11449/39165-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/39165-
dc.description.abstractThis work presents the preparation of SrBi2Nb2O9 (SBN) directly by the combustion synthesis. Strontium nitrate, niobium ammonium oxalate (NH4H2[NbO-(C2O4)(3)].3H(2)O) and bismuth oxide were used as oxidant reactants and urea as fuel. The influence of the fuel was evaluated by the addition of different fuel amounts (50%, 100%, 200% and 300%), 100% being the stoichiometric proportion. The XRD patterns showed that the SBN perovskite crystallized as the majority phase. The as-synthesized stoichiometric powder presented a specific surface area of around 13 m(2)/g and a mean grain size of around 16 nm. Dilatometric measurements showed that the maximum sintering rate occurs at 1275degreesC. The determination of the ferroparaelectric transition showed a Curie temperature (T-c) of 429degreesC. (C) 2002 Elsevier B.V. B.V. All rights reserved.en
dc.format.extent2812-2816-
dc.language.isoeng-
dc.publisherElsevier B.V.-
dc.sourceWeb of Science-
dc.subjectcombustion synthesispt
dc.subjectSrBi2Nb2O9pt
dc.subjectpowderpt
dc.subjectferroelectricpt
dc.subjectbismuth layerpt
dc.titlePreparation and characterization of nanosized SrBi2Nb2O9 powder by the combustion synthesisen
dc.typeoutro-
dc.contributor.institutionUniversidade Federal de São Carlos (UFSCar)-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.description.affiliationUFSCar CMDMC LIEC, BR-13565905 Sao Carlos, SP, Brazil-
dc.description.affiliationUNESP CMDMC LIEC, BR-14801970 Araraquara, SP, Brazil-
dc.description.affiliationUnespUNESP CMDMC LIEC, BR-14801970 Araraquara, SP, Brazil-
dc.identifier.doi10.1016/S0167-577X(02)01380-0-
dc.identifier.wosWOS:000183268500009-
dc.rights.accessRightsAcesso restrito-
dc.relation.ispartofMaterials Letters-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.