You are in the accessibility menu

Please use this identifier to cite or link to this item: http://acervodigital.unesp.br/handle/11449/63776
Full metadata record
DC FieldValueLanguage
dc.contributor.authorConforto, E.-
dc.contributor.authorRechenberg, H. R.-
dc.contributor.authorJafelicci, M.-
dc.date.accessioned2014-05-27T01:58:25Z-
dc.date.accessioned2016-10-25T18:12:07Z-
dc.date.available2014-05-27T01:58:25Z-
dc.date.available2016-10-25T18:12:07Z-
dc.date.issued1986-12-01-
dc.identifierhttp://dx.doi.org/10.1016/0022-3697(86)90149-6-
dc.identifier.citationJournal of Physics and Chemistry of Solids, v. 47, n. 12, p. 1179-1184, 1986.-
dc.identifier.issn0022-3697-
dc.identifier.urihttp://hdl.handle.net/11449/63776-
dc.identifier.urihttp://acervodigital.unesp.br/handle/11449/63776-
dc.description.abstractMössbauer spectroscopy was used to investigate the early aging stage of iron(III) hydroxide sols prepared by oxidation of Fe(CO)5 in ethanolic solution, followed by vacuum drying at room temperature. One sample was composed of amorphous particles, while two other samples were partially crystallized, either as a result of solvent change or of spontaneous aging. The main results of Mössbauer measurements in the 80-320 K temperature range are: (a) partially crystallized particles exhibit a strong, S-shaped temperature dependence of the quadrupole splitting, in contrast to a weak and linear variation for amorphous particles; (b) the recoilless fraction temperature dependence is affected by vibration of the particles as a whole, with an effective force constant which is smaller for crystallized particles than for amorphous ones. Furthermore, the former exhibit anf-factor discontinuity near 0°C, which is attributed to melting of a surface layer built up during the crystallization process. © 1986.en
dc.format.extent1179-1184-
dc.language.isoeng-
dc.sourceScopus-
dc.subjectcolloidal state-
dc.subjectIron hydroxide-
dc.subjectmicrocrystals-
dc.subjectMössbauer spectroscopy-
dc.subjectrecoilless fraction-
dc.subjectCHEMICAL REACTIONS - Oxidation-
dc.subjectSPECTROSCOPY, MOSSBAUER - Applications-
dc.subjectCOLLOIDAL STATE-
dc.subjectIRON(III) HYDROXIDE PARTICLES-
dc.subjectRECOILLESS FRACTION-
dc.subjectIRON COMPOUNDS-
dc.titleMössbauer spectroscopic study of the early crystallization stage of iron(III) hydroxide particlesen
dc.typeoutro-
dc.contributor.institutionUniversidade de São Paulo (USP)-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.description.affiliationInstituto de Física Universidade de São Paulo, C.P. 20516, 01498 Sáo Paulo-
dc.description.affiliationInstituto de Química UNESP, C.P. 174, 14800 Araraquara-
dc.description.affiliationUnespInstituto de Química UNESP, C.P. 174, 14800 Araraquara-
dc.identifier.doi10.1016/0022-3697(86)90149-6-
dc.rights.accessRightsAcesso restrito-
dc.relation.ispartofJournal of Physics and Chemistry of Solids-
dc.identifier.scopus2-s2.0-0022914338-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.