dc.contributor.authorCosta, F.B.-
dc.contributor.authorTeixeira, S.R.-
dc.contributor.authorSouza, A.E.-
dc.contributor.authorSantos, G.T.A.-
dc.date.accessioned2014-05-20T13:23:09Z-
dc.date.available2014-05-20T13:23:09Z-
dc.date.issued2009-01-01-
dc.identifierhttp://dx.doi.org/10.1590/S1517-70762009000400007-
dc.identifier.citationMatéria (Rio de Janeiro). Rede Latino-Americana de Materiais, v. 14, n. 4, p. 1146-1153, 2009.-
dc.identifier.issn1517-7076-
dc.identifier.urihttp://hdl.handle.net/11449/6945-
dc.description.abstractNumerous silicates based wastes have been produced and considered for recycling and reuse. Among them, glass cullet is one of the most common silicate wastes and has considerable volume in the cities wastes. A big amount of this waste is recycled by the glass industry but another part is dumped in the cities garbage deposits. In the last few decades there has been considerable research on the reuse of glass waste as aggregate to produce glass-ceramic, for mortars, ceramics and for cement and concrete. This work is concerned to study the reuse of one way glass bottles as aggregate to produce roof tiles (red ceramic). Two kinds of glass powder were prepared by sieving: alpha (0.088 to 0.125 mm) and beta (0.037 to 0.088 mm). Prismatic ceramic bodies (CB) were pressed (60 x 20 x ~5 mm) using a ceramic mass with 0, 5, 8 and 10 % of glass cullet powder added and fired at five different temperatures (800 to 1200 ºC). The results of the technological tests (flexural strength, water absorption, dimensional changes, density and porosity apparent) show that shrinkage increases with the glass content and all other properties above are improved. These changes are more exhibited at temperatures higher than 900°C and in the higher powder glass concentrations (8 e 10%).en
dc.description.sponsorshipFundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)-
dc.format.extent1146-1153-
dc.language.isoeng-
dc.publisherRede Latino-Americana de Materiais-
dc.sourceSciELO-
dc.subjectroof tilesen
dc.subjectglassen
dc.subjectone-way bottlesen
dc.subjectrecyclingen
dc.titleRecycling of glass cullet as aggregate for clays used to produce roof tilesen
dc.typeoutro-
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)-
dc.description.affiliationUniversidade Estadual Paulista Faculdade de Ciências e Tecnologia Departamento de Física, Química e Biologia-
dc.description.affiliationUnespUniversidade Estadual Paulista Faculdade de Ciências e Tecnologia Departamento de Física, Química e Biologia-
dc.description.sponsorshipIdFAPESP: 04/15421-2-
dc.identifier.doi10.1590/S1517-70762009000400007-
dc.identifier.scieloS1517-70762009000400007-
dc.identifier.wosWOS:000276824400007-
dc.rights.accessRightsAcesso aberto-
dc.identifier.fileS1517-70762009000400007.pdf-
dc.relation.ispartofMatéria (Rio de Janeiro)-
dc.identifier.scopus2-s2.0-77749299140-
Appears in Collections:Artigos, TCCs, Teses e Dissertações da Unesp

There are no files associated with this item.
 

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.